I've been reading about Pripp's flux for quite a while now, and finally decided to make up a batch, especially for use in kiln annealing (since it's very persistent under heat). Currently I have container that's got the chemicals (3:2:2 by weight ratio of boric acid, TSP, and borax) in water. Some of it's dissolved, and some is still a slurry; I'll add some more water and try heating it again to see if I can dissolve more of it.

Then it goes in a spray bottle, since it's applied by spray to warm metal so that it dries on contact. Should be interesting!

I've tried palladium solder on palladium a few times now, and am not thrilled with the color match (or the softness). Apparently it can't be fused, at least not by a torch, which is unfortunate. I've had recommendations of both 18k palladium white gold solder (hard) and 20-21k white gold solder for use with it; I'm not sure which I'll try for my next project. It's a pair of wedding bands, so I'm hoping for a closer color match, though I did explain to the clients that there would likely be a somewhat visible seam in the back, especially under some lights, and they're OK with that.
This account has disabled anonymous posting.
If you don't have an account you can create one now.
HTML doesn't work in the subject.
More info about formatting

Profile

afmetalsmith: (Default)
afmetalsmith

September 2011

S M T W T F S
    123
45678910
11121314151617
181920 21222324
252627282930 

Most Popular Tags

Style Credit

Expand Cut Tags

No cut tags
Page generated Mar. 16th, 2026 05:44 am
Powered by Dreamwidth Studios